Self-healing of self-compacting concretes made with blast furnace slag cements activated by crystalline admixture
by Emilio M. Takagi; Maryangela G. Lima; Paulo Helene; Ronaldo A. Medeiros-Junior
International Journal of Materials and Product Technology (IJMPT), Vol. 56, No. 1/2, 2018

Abstract: Test samples were examined using a specific crystalline admixture, AR glass fibre and three types of cements with percentages of blast furnace slag (BFS) of 55%, 35% and 0%. Test specimens were loaded under compression until 90% of their failure load, in order to generate a network of micro-cracks. These samples were subsequently immersed in lime water to trigger the self-healing mechanism, followed by various tests at 28, 56 and 84 days. As BFS content ratio was increased to 55%, there was a noticeable increase in mechanical recovery and permeation reduction properties, indicating good self-healing.

Online publication date: Sun, 07-Jan-2018

The full text of this article is only available to individual subscribers or to users at subscribing institutions.

 
Existing subscribers:
Go to Inderscience Online Journals to access the Full Text of this article.

Pay per view:
If you are not a subscriber and you just want to read the full contents of this article, buy online access here.

Complimentary Subscribers, Editors or Members of the Editorial Board of the International Journal of Materials and Product Technology (IJMPT):
Login with your Inderscience username and password:

    Username:        Password:         

Forgotten your password?


Want to subscribe?
A subscription gives you complete access to all articles in the current issue, as well as to all articles in the previous three years (where applicable). See our Orders page to subscribe.

If you still need assistance, please email subs@inderscience.com