Optimisation of porosity of 7075 Al alloy 10% SiC composite produced by stir casting process through Taguchi method
by Rajesh Kumar Bhushan, Sudhir Kumar, S. Das
International Journal of Materials Engineering Innovation (IJMATEI), Vol. 1, No. 1, 2009

Abstract: In this paper an attempt has been made to achieve a set of values of stir casting process variables that may yield optimum porosity to the 7075 Al alloy with 10% SiC composite. The effect of selected process variables on the porosity of 7075 Al alloy 10% SiC composite and subsequent optimal settings of the variables have been obtained using Taguchi method. The results indicate that the holding time, holding temperature and stirring speed are the significant variables. Stirring time is insignificant variable. As the holding time, holding temperature and stirring time increases the porosity decreases. When the stirring speed increases, porosity increases. The predicted optimal value of porosity is 4.71%.

Online publication date: Tue, 24-Mar-2009

The full text of this article is only available to individual subscribers or to users at subscribing institutions.

 
Existing subscribers:
Go to Inderscience Online Journals to access the Full Text of this article.

Pay per view:
If you are not a subscriber and you just want to read the full contents of this article, buy online access here.

Complimentary Subscribers, Editors or Members of the Editorial Board of the International Journal of Materials Engineering Innovation (IJMATEI):
Login with your Inderscience username and password:

    Username:        Password:         

Forgotten your password?


Want to subscribe?
A subscription gives you complete access to all articles in the current issue, as well as to all articles in the previous three years (where applicable). See our Orders page to subscribe.

If you still need assistance, please email subs@inderscience.com